Parameters
Product Overview: a two-component epoxy zinc-rich shop primer formulated from zinc powder, epoxy resin and polyamide curing agent
Main characteristics: 
zinc powder has a cathodic protection property and excellent rust resistance
quick drying, good heat resistance, small burning area welding 
and cutting, film thicknessdoes not affect the welding performance within the specified range
can be matched with most paint systems
Uses:as shop primer on the steel pretreatment line by shipyard, heavy machinery factory, etc. for maintenance
Color:gray, matt
Volume solid content:50±2%
Standard film thickness:20 micron by dry film (40 micron by wet film)
Theoretical coating rate:Theoretical coating rate at 20micron dry film thickness24m2/l(appropriate loss factor allowed)
Application methods: airless spray, roll coating, brushing
Flash point:5℃(mixture)
Drying time:
25℃
surface  drying ≤5min
hard  drying ≤24h
fully cured 7d
Production line drying time≤5min(steel preheating50℃, drying tunnel temperature120℃)
Painting methods:
airless spray   thinner    special thinner
dilution amount   0-5%(by paint weight)
roll coating /brushing thinner   special thinner
dilution amount   0-3%(by paint weight)
Cleaner: special thinner
Storage period:  12 months, stored in a dry and cool place, away from heat and fire
Surface treatment and substrate temperature:Oxidized steel:sand-blasting to Sa2.5;
Non-oxidized steel: sanding to St3 with elastic grinding wheel;
Steel coated with shop primer: secondary descaling for paint film damage and rust, sanding to St3;
Burnt part through welding flame cutting or flame correction: sanding to St3, the substrate temperature must be higher than the dew point 3℃
 
Notice: The zinc-rich primer surface can form zinc salt (commonly known as white rust), so it should not be exposed for a long time before the next coating. For longer coating intervals, it is recommended to apply an epoxy cloud iron primer as a sealing layer as soon as possible to reduce the amount of secondary descaling.
The surface of zinc-rich primer with zinc salt should be cleaned by sweep blasting or mechanical rust removal for secondary descaling all oil and impurities should be removed.
Dry spray is prone to occur during high temperature seasons. To prevent dry spray, the paint must be adjusted with thinner.
Cautions:During the painting and drying process, appropriate ventilation and precautions must be taken to control the solvent concentration within the safety limits to prevent the risk of poisoning or lack of oxygen. Take protective measures to prevent skin and eyes from coming into contact with the product. Specific safety measures such as gloves, goggles, and masks should be determined depending on the application method and working environment.
Scan the QR code to read on your phone
We could not find any corresponding parameters, please add them to the properties table
Next
YanTai GuangCi Coatings Co., Ltd.

Address:

Taocun economic development zone of Yantai Shandong

YanTai GuangCi Coatings Co., Ltd.

E-mail:

150168216@qq.com

Username used for comment:
Message
Description:
验证码

© YanTai GuangCi Coatings Co., Ltd.

鲁ICP备20019790号 Powered by:www.300.cn

 

YanTai GuangCi Coatings Co., Ltd.